MOT Status
ValidMileage
87,104 miSignificantly above average — investigate
Not all car check providers offer a guarantee. Don't risk buying from services that can't back their data. CarVerify reports include a £30,000 finance data guarantee.
Vehicle Details
All premium checks include
50+ data pointsMOT History
Nearside Front Anti-roll bar ball joint excessively worn (5.3.4 (a) (i))
Offside Front Anti-roll bar ball joint excessively worn (5.3.4 (a) (i))
Nearside Front Outer Tyre tread depth below requirements of 1.6mm edge (5.2.3 (e)) DANGEROUS
Offside Front Outer Tyre tread depth below requirements of 1.6mm edge (5.2.3 (e)) DANGEROUS
Battery insecure but not likely to fall from carrier (4.13 (a) (i))
Nearside Rear Tyre slightly damaged/cracking or perishing (5.2.3 (d) (ii))
Offside Rear Tyre slightly damaged/cracking or perishing (5.2.3 (d) (ii))
Front Brake disc worn, pitted or scored, but not seriously weakened (1.1.14 (a) (ii))
Nearside Front Anti-roll bar linkage ball joint has slight play (5.3.4 (a) (i))
Nearside Front Outer Tyre worn close to legal limit/worn on edge (5.2.3 (e))
Offside Front Anti-roll bar linkage ball joint has slight play (5.3.4 (a) (i))
Offside Rear Suspension component mounting prescribed area is corroded but not considered excessive rear lower arch/sill (5.3.6 (a) (i))
Offside Rear Upper Suspension component mounting prescribed area is corroded but not considered excessive upper chassis leg by the spring (5.3.6 (a) (i))
underside of car has corrosion / covered in under sill
Nearside Front Outer Track rod end ball joint has excessive play (2.1.3 (b) (i))
Nearside Rear Lower Suspension component mounting prescribed area excessively corroded significantly reducing structural strength lower rear sill/arch (in yellow chalk) below sill cover (5.3.6 (a) (i))
Nearside Rear Upper Suspension component mounting prescribed area excessively corroded significantly reducing structural strength upper chassis leg by the spring (in yellow chalk) (5.3.6 (a) (i))
Offside Front Outer Track rod end ball joint has excessive play (2.1.3 (b) (i))
Front Brake disc worn, pitted or scored, but not seriously weakened (1.1.14 (a) (ii))
Nearside Front Anti-roll bar linkage ball joint has slight play (5.3.4 (a) (i))
Nearside Front Outer Tyre worn close to legal limit/worn on edge (5.2.3 (e))
Offside Front Anti-roll bar linkage ball joint has slight play (5.3.4 (a) (i))
Offside Rear Suspension component mounting prescribed area is corroded but not considered excessive rear lower arch/sill (5.3.6 (a) (i))
Offside Rear Upper Suspension component mounting prescribed area is corroded but not considered excessive upper chassis leg by the spring (5.3.6 (a) (i))
underside of car has corrosion / covered in under sill
Front Brake disc worn, pitted or scored, but not seriously weakened (1.1.14 (a) (ii))
Nearside Front Tyre worn close to legal limit/worn on edge (5.2.3 (e))
underside of vehicle covered in underseal
Brake performance unable to be tested (1.2.1 (g))
Exhaust carbon monoxide content after 2nd fast idle exceeds manufacturer's specified limits (8.2.1.2 (a))
Offside Front Position lamp not working (4.2.1 (a) (ii))
Nearside Rear Brake pipe leaking on a hydraulic braking system (1.1.11 (b) (ii)) DANGEROUS
Front Brake disc worn, pitted or scored, but not seriously weakened (1.1.14 (a) (ii))
Nearside Front Tyre worn close to legal limit/worn on edge (5.2.3 (e))
Offside Rear Brake pipe corroded, covered in grease or other material (1.1.11 (c))
underside of vehicle covered in underseal
Front Brake disc worn, pitted or scored, but not seriously weakened (1.1.14 (a) (ii))
Nearside Front Anti-roll bar linkage ball joint has slight play (5.3.4 (a) (i))
Nearside Front Tyre worn close to legal limit/worn on edge (5.2.3 (e))
Nearside Rear Brake pipe corroded, covered in grease or other material (1.1.11 (c))
Offside Front Anti-roll bar linkage ball joint has slight play (5.3.4 (a) (i))
Offside Rear Brake pipe corroded, covered in grease or other material (1.1.11 (c))
Nearside Front Inner Suspension component mounting prescribed area excessively corroded significantly reducing structural strength sill (5.3.6 (a) (i))
Offside Front Wheel bearing has excessive play (5.1.3 (a) (i))
Offside Front Wheel bearing rough when rotated (5.1.3 (b) (i))
Offside Rear Inner Suspension component mounting prescribed area excessively corroded significantly reducing structural strength arch (5.3.6 (a) (i))
Offside Rear Inner Suspension component mounting prescribed area excessively corroded significantly reducing structural strength sill (5.3.6 (a) (i))
Front Brake disc worn, pitted or scored, but not seriously weakened (1.1.14 (a) (ii))
Nearside Front Anti-roll bar linkage ball joint has slight play (5.3.4 (a) (i))
Nearside Front Tyre worn close to legal limit/worn on edge (5.2.3 (e))
Nearside Rear Brake pipe corroded, covered in grease or other material (1.1.11 (c))
Offside Front Anti-roll bar linkage ball joint has slight play (5.3.4 (a) (i))
Offside Rear Brake pipe corroded, covered in grease or other material (1.1.11 (c))
Nearside Front Inner Cab or chassis has excessive corrosion, seriously affecting its strength within 30cm of a cab mounting (6.2.2 (d) (i))
Offside Front Wheel bearing rough when rotated has play to (5.1.3 (b) (i))
Offside Rear Inner Vehicle structure or chassis has excessive corrosion, seriously affecting its strength within 30cm of a body mounting (6.2.2 (d) (i))
Front Brake pipe corroded, covered in grease or other material (1.1.11 (c))
Nearside Front Tyre worn close to legal limit/worn on edge outer edge (5.2.3 (e))
Oil leak, but not excessive (8.4.1 (a) (i))
Power steering pipe/hose slightly corroded (2.1.5 (g) (i))
Rear Brake pipe corroded, covered in grease or other material runs across rear axle (1.1.11 (c))
corrosion across underside of vehicle
Anti-lock braking system warning lamp indicates an ABS fault (1.6 (b))
Exhaust Lambda reading after 2nd fast idle outside specified limits (8.2.1.2 (c))
Nearside Rear Vehicle structure corroded to the extent that the rigidity of the assembly is significantly reduced (6.1.1 (c) (i))
Offside Rear Vehicle structure corroded to the extent that the rigidity of the assembly is significantly reduced (6.1.1 (c) (i))
Exhaust has a minor leak of exhaust gases (6.1.2 (a))
Front Brake pipe corroded, covered in grease or other material (1.1.11 (c))
Nearside Front Tyre worn close to legal limit/worn on edge outer edge (5.2.3 (e))
Oil leak, but not excessive (8.4.1 (a) (i))
Power steering pipe/hose slightly corroded (2.1.5 (g) (i))
Rear Brake pipe corroded, covered in grease or other material runs across rear axle (1.1.11 (c))
corrosion across underside of vehicle
Nearside Rear body mount corroded.
Nearside Track rod end ball joint has slight play (2.1.3 (b) (i))
Offside Rear body mount corroded.
exhaust system corroded.
Exhaust has a minor leak of exhaust gases (7.1.2)
Offside front brake binding (3.7.B.1)
Nearside Inner Seat belt anchorage prescribed area is excessively corroded (5.2.6)
Offside Rear Suspension component mounting prescribed area is excessively corroded (2.4.A.3)
Offside Seat belt anchorage prescribed area is excessively corroded (5.2.6)
Lower Body has slight corrosion (6.1.B.2)
Lower Vehicle structure has slight corrosion (6.1.B.2)
Nearside Front Headlamp aim too high (1.8)
Lower Body has slight corrosion (6.1.B.2)
Lower Vehicle structure has slight corrosion (6.1.B.2)
n/s/f slight bind on brakes
Nearside Side repeater missing (1.4.A.2b)
Offside Windscreen wiper does not clear the windscreen effectively (8.2.2)
Rear Exhaust has part of the system excessively deteriorated (7.1.1a)
n/s/f slight bind on brakes
Rear Exhaust has part of the system slightly deteriorated (7.1.1a)
Exhaust emissions carbon monoxide content after 2nd fast idle excessive (7.3.D.3)
Exhaust has part of the system slightly deteriorated (7.1.1a)
How Reliable is the Suzuki Jimny?
Based on 677,512 MOT tests across 43,507 vehicles.
Top MOT Failure Points
Don't risk it. Know before you buy.
Not all vehicle check providers are the same. Some don't offer a data guarantee, which means if their information is wrong, you're on your own. Every CarVerify report is backed by a £30,000 finance data guarantee.
DU54 MOV is a 2004 Suzuki Jimny in Red with a 1,298cc petrol engine. This vehicle has been through 30 MOT tests with a personal pass rate of 60%.
Across all 2004 Suzuki Jimny models, the average MOT pass rate is 75.5% with a typical mileage of 55,220 miles. This particular vehicle has a lower pass rate than the average for its year, which may indicate maintenance issues worth investigating.
The most common reason a Suzuki Jimny fails its MOT is brake pipe excessively corroded, accounting for 18,210 recorded failures. If you're considering buying DU54 MOV, it's worth having these areas checked by a mechanic before committing.
The Suzuki Jimny typically stays on UK roads for around 28 years. At 22 years old, this Suzuki Jimny is well into its expected lifespan but still has years ahead.
Frequently Asked Questions
How do I check the history of DU54 MOV?
You can check the full history of DU54 MOV by running a full vehicle check. This shows you finance, stolen, write-off, MOT history, mileage records and more.
What year was DU54 MOV registered?
DU54 MOV is a 2004 Suzuki Jimny, first registered on 13 September 2004.
Is DU54 MOV safe to buy?
The MOT history for DU54 MOV shows 30 tests with a 60% pass rate. To check for outstanding finance, stolen markers, write-off history and mileage discrepancies, run a full vehicle check.
Does DU54 MOV have outstanding finance?
Finance checks require a premium vehicle report. This checks against all major UK finance providers to see if there is any outstanding finance on DU54 MOV. If you buy a car with outstanding finance, the finance company can repossess it.
No warranty or guarantee of accuracy is provided for any free data on this page. The data guarantee applies only to information obtained through the purchase of a full check.