Nearside Rear Coil spring corroded (5.3.1 (b) (i))
Offside Rear Coil spring corroded (5.3.1 (b) (i))
Offside Rear Tyre slightly damaged/cracking or perishing (5.2.3 (d) (ii))
Offside Rear Tyre worn close to legal limit/worn on edge (5.2.3 (e))
Nearside Front Coil spring fractured or broken (5.3.1 (b) (i))
Nearside Rear Coil spring corroded (5.3.1 (b) (i))
Offside Rear Coil spring corroded (5.3.1 (b) (i))
Offside Rear Tyre slightly damaged/cracking or perishing (5.2.3 (d) (ii))
Offside Rear Tyre worn close to legal limit/worn on edge (5.2.3 (e))
TPMS Light On
Front Inner Brake disc worn, pitted or scored, but not seriously weakened (1.1.14 (a) (ii))
Nearside Rear Coil spring corroded (5.3.1 (b) (i))
Offside Rear Coil spring corroded (5.3.1 (b) (i))
Offside Rear Tyre slightly damaged/cracking or perishing (5.2.3 (d) (ii))
Offside Rear Tyre worn close to legal limit/worn on edge (5.2.3 (e))
TPMS Light On
Offside Front Inner Brake disc worn, pitted or scored, but not seriously weakened (1.1.14 (a) (ii))
Offside Rear Tyre slightly damaged/cracking or perishing (5.2.3 (d) (ii))
TPMS Light On
Nearside Front Tyre has a cut in excess of the requirements deep enough to reach the ply or cords (5.2.3 (d) (i))
Nearside Front Tyre tread depth below requirements of 1.6mm (5.2.3 (e)) DANGEROUS
Offside Front Inner Brake disc worn, pitted or scored, but not seriously weakened (1.1.14 (a) (ii))
Offside Rear Tyre slightly damaged/cracking or perishing (5.2.3 (d) (ii))
TPMS Light On
Nearside Front Tyre slightly damaged/cracking or perishing (5.2.3 (d) (ii))
Nearside Rear Tyre slightly damaged/cracking or perishing (5.2.3 (d) (ii))
Front Registration plate missing (0.1 (a))
Rear Registration plate missing (0.1 (a))
Nearside Front Tyre slightly damaged/cracking or perishing (5.2.3 (d) (ii))
Nearside Rear Tyre slightly damaged/cracking or perishing (5.2.3 (d) (ii))
Surface corrosion on inside of all brake discs.
Rear Inner brake disc worn, pitted or scored, but not seriously weakened faces (3.5.1i)
tpms light on
all brake discs slight pitting inner face
brake flexy pipes slight corrosion on solid part
Nearside Rear Tyre worn close to the legal limit (4.1.E.1)
Offside Rear Tyre worn close to the legal limit (4.1.E.1)
TPM WARN LIGHT ON
Under-trays fitted obscuring some underside components
all four tyres small cracks in road face
front discs slight pitting
rear discs pitting
Engine covers fitted obscuring some components in the engine bay
Under-trays fitted obscuring some underside components
O/S front tyre wearing on outer edge
Nearside Front coil spring fractured (2.4.C.1a)
Offside Front coil spring fractured (2.4.C.1a)
O/S front tyre wearing on outer edge
Rear rear brake binding (3.7.B.1)
front flexy pipes on both sides slight corrosion on metal
front tyres slight wear on edges
How Reliable is the Aston Martin DB9?
Based on 83,149 MOT tests across 5,749 vehicles.
Top MOT Failure Points
Don't risk it. Know before you buy.
Not all vehicle check providers are the same. Some don't offer a data guarantee, which means if their information is wrong, you're on your own. Every CarVerify report is backed by a £30,000 finance data guarantee.
DW04 SET is a 2007 Aston Martin DB9 in Silver with a 5,935cc petrol engine. This vehicle has been through 20 MOT tests with a personal pass rate of 75%.
Across all 2007 Aston Martin DB9 models, the average MOT pass rate is 89.7% with a typical mileage of 28,357 miles. This particular vehicle has a lower pass rate than the average for its year, which may indicate maintenance issues worth investigating.
The most common reason a Aston Martin DB9 fails its MOT is position lamp(s) not working, accounting for 649 recorded failures. If you're considering buying DW04 SET, it's worth having these areas checked by a mechanic before committing.
The Aston Martin DB9 typically stays on UK roads for around 22 years. At 19 years old, this Aston Martin DB9 is approaching the upper end of the typical lifespan for this model.
Frequently Asked Questions
How do I check the history of DW04 SET?
You can check the full history of DW04 SET by running a full vehicle check. This shows you finance, stolen, write-off, MOT history, mileage records and more.
What year was DW04 SET registered?
DW04 SET is a 2007 Aston Martin DB9, first registered on 4 July 2007.
Is DW04 SET safe to buy?
The MOT history for DW04 SET shows 20 tests with a 75% pass rate. To check for outstanding finance, stolen markers, write-off history and mileage discrepancies, run a full vehicle check.
Does DW04 SET have outstanding finance?
Finance checks require a premium vehicle report. This checks against all major UK finance providers to see if there is any outstanding finance on DW04 SET. If you buy a car with outstanding finance, the finance company can repossess it.
No warranty or guarantee of accuracy is provided for any free data on this page. The data guarantee applies only to information obtained through the purchase of a full check.