MOT Status
ValidMileage
119,339 miSignificantly above average — investigate
Not all car check providers offer a guarantee. Don't risk buying from services that can't back their data. CarVerify reports include a £30,000 finance data guarantee.
Vehicle Details
All premium checks include
50+ data pointsMOT History
Exhaust has a major leak of exhaust gases (6.1.2 (a))
Rear Exhaust silencer likely to become detached Due to corrosion and fracture (8.1.1 (b) (ii)) DANGEROUS
Front Brake disc worn, pitted or scored, but not seriously weakened (1.1.14 (a) (ii))
Front Brake pad(s) wearing thin (1.1.13 (a) (ii))
Offside Front Lower Suspension arm ball joint has slight play track control arm (5.3.4 (a) (i))
Nearside Front Brake pipe corroded, covered in grease or other material to rear rusting by fuel tank (1.1.11 (c))
Nearside Rear Brake hose slightly deteriorated (1.1.12 (b) (ii))
Nearside Rear parking brake efficiency low
Offside Front Brake pipe corroded, covered in grease or other material to rear rusting by fuel tank (1.1.11 (c))
Offside Rear Brake hose slightly deteriorated (1.1.12 (b) (ii))
Nearside Front Brake hose excessively deteriorated (1.1.12 (b) (ii))
Offside Front Brake hose excessively deteriorated (1.1.12 (b) (ii))
Nearside Front Brake pipe corroded, covered in grease or other material to rear rusting by fuel tank (1.1.11 (c))
Nearside Rear Brake hose slightly deteriorated (1.1.12 (b) (ii))
Nearside Rear parking brake efficiency low
Nearside Wheel bearing has slight play (5.1.3 (a) (i))
Offside Front Brake pipe corroded, covered in grease or other material to rear rusting by fuel tank (1.1.11 (c))
Offside Rear Brake hose slightly deteriorated (1.1.12 (b) (ii))
Nearside Front Lower Suspension arm pin or bush worn but not resulting in excessive movement (5.3.4 (a) (i))
Nearside Front Wheel bearing has slight play (5.1.3 (a) (i))
Nearside Rear Brake pipe corroded, covered in grease or other material (1.1.11 (c))
Nearside Rear Upper Suspension arm corroded but not seriously weakened radius arm (5.3.3 (b) (i))
Offside Front Lower Suspension arm pin or bush worn but not resulting in excessive movement both arms (5.3.4 (a) (i))
Offside Front Wheel bearing has slight play (5.1.3 (a) (i))
Offside Rear Upper Suspension arm corroded but not seriously weakened radius arm (5.3.3 (b) (i))
Rear Sub-frame corroded but not seriously weakened (5.3.3 (b) (i))
Nearside Rear Coil spring corroded (5.3.1 (b) (i))
Offside Rear Coil spring corroded (5.3.1 (b) (i))
Nearside Rear Brake pipe excessively corroded (1.1.11 (c))
Offside Rear Brake pipe excessively corroded (1.1.11 (c))
Nearside Rear Coil spring corroded (5.3.1 (b) (i))
Offside Front Tyre worn close to legal limit/worn on edge just legal on the inside edge (5.2.3 (e))
Offside Rear Coil spring corroded (5.3.1 (b) (i))
Nearside Rear Brake pipe corroded, covered in grease or other material Close to brake hose and above rear of fuel tank (1.1.11 (c))
Nearside Rear Coil spring corroded (5.3.1 (b) (i))
Nearside Rear Tyre worn close to legal limit/worn on edge 205 55 16 3mm (5.2.3 (e))
Offside Rear Coil spring corroded (5.3.1 (b) (i))
Nearside Front Upper Anti-roll bar linkage ball joint dust cover no longer prevents the ingress of dirt (5.3.4 (b) (ii))
Offside Front Upper Anti-roll bar linkage ball joint dust cover no longer prevents the ingress of dirt (5.3.4 (b) (ii))
Windscreen wiper does not clear the windscreen effectively (3.4 (b) (ii))
Nearside Rear Brake pipe corroded, covered in grease or other material Close to brake hose and above rear of fuel tank (1.1.11 (c))
Nearside Rear Coil spring corroded (5.3.1 (b) (i))
Nearside Rear Tyre worn close to legal limit/worn on edge 205 55 16 3mm (5.2.3 (e))
Offside Rear Coil spring corroded (5.3.1 (b) (i))
Brake pipe corroded, covered in grease or other material All (1.1.11 (c))
Offside Rear Brake pipe corroded, covered in grease or other material 2 pipes corroded (1.1.11 (c))
Nearside Rear Coil spring corroded (5.3.1 (b) (i))
Offside Rear Coil spring corroded (5.3.1 (b) (i))
rear coil springs corroded
Nearside Front Suspension arm rubber bush deteriorated but not resulting in excessive movement (2.4.G.2)
Nearside Front tyre outer side wall damage
Nearside Rear coil spring corroded (2.4.C.1b)
Offside Front Suspension arm rubber bush deteriorated but not resulting in excessive movement (2.4.G.2)
Offside Rear coil spring corroded (2.4.C.1b)
Nearside Rear Brake pad(s) wearing thin (3.5.1g)
Offside Rear Brake pad(s) wearing thin (3.5.1g)
Offside Rear coil spring corroded (2.4.C.1b)
Nearside Rear Brake pad(s) wearing thin (3.5.1g)
Offside Rear Brake pad(s) wearing thin (3.5.1g)
Offside Rear coil spring corroded (2.4.C.1b)
Offside Rear Tyre worn close to the legal limit (4.1.E.1)
Offside Rear coil spring corroded (2.4.C.1b)
Offside Obligatory mirror insecure (8.1.1)
Non obligatory mirror damaged
Offside Rear Tyre worn close to the legal limit (4.1.E.1)
Offside Rear coil spring corroded (2.4.C.1b)
Nearside Rear Tyre worn close to the legal limit (4.1.E.1)
offside front tyre worn heavily on inner edge
srs light on
Offside Front Anti-roll bar linkage ball joint dust cover excessively damaged so that it no longer prevents the ingress of dirt (2.4.G.2)
Nearside Rear Tyre worn close to the legal limit (4.1.E.1)
offside front tyre worn heavily on inner edge
srs light on
Nearside Front Tyre worn close to the legal limit (4.1.E.1)
n/s/f tyer worn close to cord outeredge
How Reliable is the Mercedes-benz C?
Based on 8,031,355 MOT tests across 683,668 vehicles.
Top MOT Failure Points
Don't risk it. Know before you buy.
Not all vehicle check providers are the same. Some don't offer a data guarantee, which means if their information is wrong, you're on your own. Every CarVerify report is backed by a £30,000 finance data guarantee.
GV56 ORW is a 2007 Mercedes-benz C in Blue with a 1,796cc petrol engine. This vehicle has been through 23 MOT tests with a personal pass rate of 73.9%.
Across all 2007 Mercedes-benz C models, the average MOT pass rate is 76.0% with a typical mileage of 79,646 miles. This particular vehicle has a lower pass rate than the average for its year, which may indicate maintenance issues worth investigating.
The most common reason a Mercedes-benz C fails its MOT is tyre tread depth below requirements of 1.6mm, accounting for 240,078 recorded failures. If you're considering buying GV56 ORW, it's worth having these areas checked by a mechanic before committing.
The Mercedes-benz C typically stays on UK roads for around 32 years. At 19 years old, this Mercedes-benz C is well into its expected lifespan but still has years ahead.
Frequently Asked Questions
How do I check the history of GV56 ORW?
You can check the full history of GV56 ORW by running a full vehicle check. This shows you finance, stolen, write-off, MOT history, mileage records and more.
What year was GV56 ORW registered?
GV56 ORW is a 2007 Mercedes-benz C, first registered on 16 January 2007.
Is GV56 ORW safe to buy?
The MOT history for GV56 ORW shows 23 tests with a 73.9% pass rate. To check for outstanding finance, stolen markers, write-off history and mileage discrepancies, run a full vehicle check.
Does GV56 ORW have outstanding finance?
Finance checks require a premium vehicle report. This checks against all major UK finance providers to see if there is any outstanding finance on GV56 ORW. If you buy a car with outstanding finance, the finance company can repossess it.
No warranty or guarantee of accuracy is provided for any free data on this page. The data guarantee applies only to information obtained through the purchase of a full check.